this post was submitted on 13 Jan 2026
30 points (100.0% liked)

3DPrinting

20903 readers
68 users here now

3DPrinting is a place where makers of all skill levels and walks of life can learn about and discuss 3D printing and development of 3D printed parts and devices.

The r/functionalprint community is now located at: or !functionalprint@fedia.io

There are CAD communities available at: !cad@lemmy.world or !freecad@lemmy.ml

Rules

If you need an easy way to host pictures, https://catbox.moe/ may be an option. Be ethical about what you post and donate if you are able or use this a lot. It is just an individual hosting content, not a company. The image embedding syntax for Lemmy is ![](URL)

Moderation policy: Light, mostly invisible

founded 2 years ago
MODERATORS
 

After Having experimented in Making Perfectly Smooth Surfaces for about a Year now within the Print Process itself, Its time I Capitulate and start putting in some more Work and Sand it all smooth!

Just a bit of an Issue... Whenever I sand Coloured PETG, it looses its Colour and turns into that Broken Plastic White.

As someone who hasn't had to Fix something like that before, I'm not sure where to even start Fixing this? Can it be Avoided in the Sanding Process, or can the Colour be Regained afterwards?

I have heard of People Treating it with Heat and Vasaline to get the Colour Back, what kind of Methods do you all use and how reliable are they?

you are viewing a single comment's thread
view the rest of the comments
[–] Mr_Mofu@lemmy.blahaj.zone 2 points 2 days ago (1 children)

I have tried using a Regular Soldering Iron to smooth out the surfaces, to not a lotta luck tho. At what temps can the Plastic Colouring be regained? Because I think I had mine set too high

[–] Tolookah@discuss.tchncs.de 1 points 2 days ago* (last edited 2 days ago)

I've used my soldering iron at 200c to re-attach broken off pieces, to much success.