this post was submitted on 19 Jan 2026
20 points (100.0% liked)

3DPrinting

21318 readers
25 users here now

3DPrinting is a place where makers of all skill levels and walks of life can learn about and discuss 3D printing and development of 3D printed parts and devices.

The r/functionalprint community is now located at: or !functionalprint@fedia.io

There are CAD communities available at: !cad@lemmy.world or !freecad@lemmy.ml

Rules

If you need an easy way to host pictures, https://catbox.moe/ may be an option. Be ethical about what you post and donate if you are able or use this a lot. It is just an individual hosting content, not a company. The image embedding syntax for Lemmy is ![](URL)

Moderation policy: Light, mostly invisible

founded 2 years ago
MODERATORS
 

I've had a MK4S for over a week now, and 100% of the prints I've tried to make on the textured sheets have partially or totally failed. PLA prints beautifully on the smooth sheet, but PLA, PETG and ABS, I think I could print on the surface of a 10 inch tank of oil with more success than the textured sheet. Plastic doesn't stick to it. I've wiped it with isopopyl, I've washed it with dawn...it's a bad print surface and I want my money back.

you are viewing a single comment's thread
view the rest of the comments
[–] emenl@lemmy.world 14 points 2 weeks ago (17 children)

I had issues with mine, nothing was sticking to it causing 100% failures. I forgot where I read it but I ended up scrubbing it good with one of those slightly abrasive green pads in warm dawn dish soap, drying it with a clean microfiber cloth and putting it on the bed with the heat set to 60c for a few minutes. It now works extremely well with pla or petg, I just wipe it down with a bit of 90% alcohol between prints. Never had any issues with the smooth and satin sheets.

[–] captain_aggravated@sh.itjust.works 5 points 2 weeks ago* (last edited 2 weeks ago) (15 children)

Kitchen sink washed and rinsed. Water run as hot as I can get it this time of year. Drain plug installed, textured sheet washed with a fresh green Scotchbrite pad under hot water and Dawn dish soap. Each side scoured in horizontal strokes, vertical strokes, diagonal top-left to bottom-right strokes, diagonal top-right to bottom-left strokes, in counter-clockwidse circles in horizontal strokes, and clockwise circles in vertical strokes. Repeated 3 times each side. Dried with laundered microfiber cloth. Placed on printer heat bed and heated to 60C for 5 minutes per side.

This makes the 4th, 5th and 6th time this sheet they tell you not to submerge in water has been washed in a sink full of soap and water.

Brand new spool of Printed Solid Jessie PETG filament loaded, corresponding filament preset selected in slicer. Tool caddy with assistant discs at sharp corners sliced, sent to printer, Z offset set at -0.025mm, 1 glencairn of small batch 90 proof straight bourbon poured...

Edit:

[–] IMALlama@lemmy.world 1 points 2 weeks ago

Seems like great success? If so, great. The only things about your routine I would change is to not submerge, not because that's bad but because who wants to obsess over cleaning their sink first, and use paper towels to dry. You want to make sure no films are transferred to the bed.