this post was submitted on 16 Jan 2026
18 points (95.0% liked)

3DPrinting

21026 readers
184 users here now

3DPrinting is a place where makers of all skill levels and walks of life can learn about and discuss 3D printing and development of 3D printed parts and devices.

The r/functionalprint community is now located at: or !functionalprint@fedia.io

There are CAD communities available at: !cad@lemmy.world or !freecad@lemmy.ml

Rules

If you need an easy way to host pictures, https://catbox.moe/ may be an option. Be ethical about what you post and donate if you are able or use this a lot. It is just an individual hosting content, not a company. The image embedding syntax for Lemmy is ![](URL)

Moderation policy: Light, mostly invisible

founded 2 years ago
MODERATORS
 

I'm about to paint a PLA 3D print for the first time, and while there is some advice on what primer to use (an automotive etching plastic primer seems to be it), I've not see anything but hand wavy "add a layer of clear coat" for sealing.

Does anyone have any advice on a matte finish clear coat product that works well, as much so I know I have the right class/type of product?

Also, is there much difference between the products from hobby shops vs hardware stores? I can imagine the hobby ones are at a consistency for painting fine details, but it may also all be the same thing.

Thanks

you are viewing a single comment's thread
view the rest of the comments
[–] otter@lemmy.dbzer0.com 1 points 6 days ago* (last edited 6 days ago)

No worries, that seems fairly straightforward overall in that the abutting hinge surfaces could go unvarnished but sanded, (I'd use dot stickers, if you don't feel like fiddling w/ hand-cut tape pieces) followed by a light dusting of graphite (ie. shave some pencil lead into a creased post-it and then sift it onto them [and into the rod's channel, for inc. smooth action]). The rest can be clear coated to your preference. (leave said masking on until this step is complete & dry cured, fyi [24+ hrs])

FWIW, gloss first and then matte for super durability as IIRC, the gloss particulate is torus-shaped whereas the matte is spheroid, and this method nests them neatly for a better bond. It's how I've sealed my TTRPG pieces for decades, and while possibly anecdotal, the results are night & day in my experience. 🤘🏼